| 项目 | 热风炉用红柱石砖 | ||
| H55 | H62 | H65 | |
| Al2O3 (%) | ≧55 | ≧62 | ≧65 |
| Fe2O3 (%) | ≦1.2 | ≦1.2 | ≦1.2 |
| 显气孔率 (%) | ≦17 | ≦17 | ≦17 |
| 体积密度 (g/cm3) | ≧2.45 | ≧2.5 | ≧2.5 |
| 常温耐压强度 (MPa) | ≧60 | ≧60 | ≧60 |
| 蠕变率 20-50h/0.2Mpa, (%) | 1350°C | 1400°C | 1450°C |
| ﹤0.2 | ﹤0.2 | ﹤0.2 | |
| 荷重软化温度 (°C) | ≧1600 | ≧1650 | ≧1680 |
| 热膨胀系数 (1000°C) (%) | ≦0.55 | ≦0.55 | ≦0.55 |